International MES research in space-technology with focus on space-applications, transportation. Aluminum 7075 aircraft wing tanks failed in the 1950s. Investigation (visual inspection, biological analysis, and chem...

Generated by MESSAI extraction pipeline · review against source PDF

Extraction

Reported parameters

No values extracted from this paper yet.

No 3D model is mapped to this paper yet. Parameter ranges above still place reported values on the literature distribution.

Abstract

Aluminum 7075 aircraft wing tanks failed in the 1950s. Investigation (visual inspection, biological analysis, and chemical analysis) supported the conclusion that MIC was the cause of the failures. Water condensed into the fuel tanks during flight led to microbial growth on the jet fuel. Pitting attack occurred under microbial deposits on the metal surface in the water phase or at the water-fuel interface. Previously, exposure of aluminum 7075 to cultures of various isolates showed that 27 bacterial isolates and 3 fungi could seriously corrode the aluminum alloy over several weeks. No recommendations were made.

Keywords

AluminiumJet fuelFuel tankAlloyCorrosionMetallurgy