MES research in electrode, membrane. The Ti/SnO 2 -Sb 2 O 3 /PbO<jats:su...

Generated by MESSAI extraction pipeline · review against source PDF

Extraction

Reported parameters

4 extracted values

View extracted values

No 3D model is mapped to this paper yet. Parameter ranges above still place reported values on the literature distribution.

Abstract

The Ti/SnO 2 -Sb 2 O 3 /PbO 2 electrodes were prepared by thermal decomposition method and its application in the electrochemical degradation of a heteropolyaromatic dye, Methylene blue (MB), contained in simulated dye wastewater were investigated under mild conditions. The effects of pH, current density and electrolysis time on de-colorization efficiency were also studied. Chemical oxygen demand (COD) was selected as another parameter to evaluate the efficiency of this degradation method on treatment of MB wastewater. The results revealed that when initial pH was 6.0, current density was 50 mA·cm 2 , electrolysis time was 60 min, Na 2 SO 4 as electrolyte and its concentration was 3.0 g·dm 3 , the de-colorization and COD removal efficiency can reach 89.9% and 71.7%, respectively.

Keywords

ElectrolysisChemical oxygen demandWastewaterElectrochemistryMethylene blueElectrolyte

Identifiers

Journal
Advanced Materials Research
Year
2012