Forschungsdaten – Titel und Zusammenfassungen von Publikationen, extrahierte Daten und Katalogeinträge – erscheinen in ihrer Originalsprache Englisch.
Publikation
Platinized Titanium as Alternative Cost‐Effective Anode for Efficient Kolbe Electrolysis in Aqueous Electrolyte Solutions
Zusammenfassung
Was die Publikation berichtet, in ihren eigenen Worten.
Zusammenfassung
Five commercial materials were assessed for electrochemical conversion of n ‐hexanoic acid by Kolbe electrolysis. Platinized titanium performed best, achieving a coulombic efficiency (CE) of 93.1±6.7 % ( n =6) for the degradation of n ‐hexanoic acid and 48.3±3.2 % ( n =6) for the production of n ‐decane, which is close to the performance of pure platinum (89.7±14.4 and 55.5±3.5 %; n =6). 56.7 mL liquid fuel was produced per mole n ‐hexanoic acid, converting to an energy demand of 6.66 kWh and 1.22 € per L. Using optical profilometry and scanning electron microscopy coupled with energy‐dispersive X‐ray spectroscopy, it was shown that the degree of coverage of the titanium surface with platinum played the most important role. An uncovered surface of as little as 1–3 % already led to a deterioration of the CE of approximately 50 %. Using platinized titanium requires >36 times less capital expenditure at only <10 % increased operational expenditure; an electrode lifetime of 10000 h can be expected.
Extrahierte Werte
Jeder aus der Publikation entnommene Wert mit seiner Quelle, damit sich jede Zahl am Text prüfen lässt.
n = 61 extrahierte Werte
Wählen Sie eine Quellenangabe, um Zitat, Seite und Konfidenz hinter einem Wert zu sehen.
0 von 61 extrahierten Zeilen modellierbar
- 61 nicht kanonisiert (kein kanonischer Slug)
| Parameter | Wert | Einheit | Konfidenz | Quelle | Anmerkungen | Modellierbar |
|---|---|---|---|---|---|---|
| Working volume of anode chamber | 200 | mL | 100 % | extrahiert | "The working volume of the anode chamber was 200 mL and that of the cathode chamb…" · cell=two-chamber, fumasep FKS-PET-130 ion exchange membrane | Ausgeschlossen: nicht kanonisiert (kein kanonischer Slug) |
| Distance between working and counter electrode | 18 | mm | 100 % | extrahiert | "keeping the WE and the CE chamber in a defined position with a 18 mm distance be…" · cell=electrode holder, three-neck 250 mL flask | Ausgeschlossen: nicht kanonisiert (kein kanonischer Slug) |
| Working volume of cathode chamber | 9 | mL | 100 % | extrahiert | "The working volume of the anode chamber was 200 mL and that of the cathode chamb…" · cell=two-chamber, fumasep FKS-PET-130 ion exchange membrane | Ausgeschlossen: nicht kanonisiert (kein kanonischer Slug) |
| Working electrode geometric surface area | 2 | cm² | 100 % | extrahiert | "a WE with a geometric surface area of 2 cm2" · electrode=working electrode (WE) | Ausgeschlossen: nicht kanonisiert (kein kanonischer Slug) |
| Current density (galvanostatic), electrode screening | 150 | mA cm⁻² | 100 % | extrahiert | "Overview of different anode materials for Kolbe electrolysis of n-hexanoic acid …" · cell=two-chamber, time=4 h, acids=["n-hexanoic acid"], electrolyte=0.25 m Na2SO4, pH 7 | Ausgeschlossen: nicht kanonisiert (kein kanonischer Slug) |
| Charge transferred per experiment | 0,44 | Faraday equivalents | 100 % | extrahiert | "Since all experiments were carried out galvanostatically, Qtotal was always 4320…" · cell=two-chamber, time=4 h, acids=["n-hexanoic acid"], electrolyte=0.25 m Na2SO4, pH 7 | Ausgeschlossen: nicht kanonisiert (kein kanonischer Slug) |
| Constant current applied | 300 | mA | 100 % | extrahiert | "The electrolysis was carried out for 4 h with a constant current of 300 mA at ro…" · cell=two-chamber, time=4 h, acids=["n-hexanoic acid"], electrolyte=0.25 m Na2SO4, pH 7 | Ausgeschlossen: nicht kanonisiert (kein kanonischer Slug) |
| Total charge passed (Qtotal) | 4.320 | C | 100 % | extrahiert | "Since all experiments were carried out galvanostatically, Qtotal was always 4320…" · cell=two-chamber, time=4 h, acids=["n-hexanoic acid"], electrolyte=0.25 m Na2SO4, pH 7 | Ausgeschlossen: nicht kanonisiert (kein kanonischer Slug) |
| Initial pH of reaction solution | 7 | — | 100 % | extrahiert | "the pH of the solution was adjusted to pH=7 using NaOH pellets and H2SO4" · acids=["n-hexanoic acid"], electrolyte=0.25 mol L−1 Na2SO4 | Ausgeschlossen: nicht kanonisiert (kein kanonischer Slug) |
| Stirring speed of anode chamber solution | 1.000 | rpm | 100 % | extrahiert | "The electrolysis was carried out for 4 h with a constant current of 300 mA at ro…" · cell=two-chamber, time=4 h, acids=["n-hexanoic acid"], electrolyte=0.25 m Na2SO4, pH 7 | Ausgeschlossen: nicht kanonisiert (kein kanonischer Slug) |
| Na2SO4 supporting electrolyte concentration | 0,25 | mol L⁻¹ | 100 % | extrahiert | "The conductivity was adjusted by adding Na2SO4 to a concentration of 0.25 mol L-…" · acids=["n-hexanoic acid"], cation=Na+ | Ausgeschlossen: nicht kanonisiert (kein kanonischer Slug) |
| Electrolysis time | 4 | h | 100 % | extrahiert | "The electrolysis was carried out for 4 h with a constant current of 300 mA at ro…" · cell=two-chamber, time=4 h, acids=["n-hexanoic acid"], electrolyte=0.25 m Na2SO4, pH 7 | Ausgeschlossen: nicht kanonisiert (kein kanonischer Slug) |
| Pt concentration in aqueous phase after electrolysis (cPt), platinized Ti Type A | 99 ±10.03 | ng mL⁻¹ | 95 % | icp-ms | "platinized Ti Type A (n=3) | 99.00±10.03" · cell=two-chamber, time=4 h, acids=["n-hexanoic acid"], electrode=platinized Ti Type A | Ausgeschlossen: nicht kanonisiert (kein kanonischer Slug) |
| Pt concentration in aqueous phase after electrolysis (cPt), platinized Ti Type B | 25,9 ±3.83 | ng mL⁻¹ | 95 % | icp-ms | "platinized Ti Type B (n=6) | 25.85±3.83" · cell=two-chamber, time=4 h, acids=["n-hexanoic acid"], electrode=platinized Ti Type B | Ausgeschlossen: nicht kanonisiert (kein kanonischer Slug) |
| Selectivity for n-decane production (S decane), platinized Ti Type A | 63,9 ±2.3 | % | 95 % | extrahiert | "platinized Ti Type A (n=3) | 77.2±51.4 | 60.4±43.0 | 63.9±2.3" · cell=two-chamber, time=4 h, acids=["n-hexanoic acid"], electrode=platinized Ti Type A | Ausgeschlossen: nicht kanonisiert (kein kanonischer Slug) |
| Selectivity for n-decane production (S decane), Pt/Ir on Ti | 49,9 ±17.5 | % | 95 % | extrahiert | "Pt/Ir on Ti (n=3) | 31.2±67.6 | 21.2±52.6 | 49.9±17.5" · cell=two-chamber, time=4 h, acids=["n-hexanoic acid"], electrode=Pt/Ir on Ti | Ausgeschlossen: nicht kanonisiert (kein kanonischer Slug) |
| Selectivity for n-decane production (S decane), platinized Ti Type B | 66,9 ±0.9 | % | 95 % | extrahiert | "platinized Ti Type B (n=6) | 65.0±7.5 | 52.3±6.9 | 66.9±0.9" · cell=two-chamber, time=4 h, acids=["n-hexanoic acid"], electrode=platinized Ti Type B | Ausgeschlossen: nicht kanonisiert (kein kanonischer Slug) |
| Pt concentration in aqueous phase after electrolysis (cPt), pure Pt | 24,6 ±9.47 | ng mL⁻¹ | 95 % | icp-ms | "pure Pt (n=3) | 24.63±9.47" · cell=two-chamber, time=4 h, acids=["n-hexanoic acid"], electrode=pure Pt foil | Ausgeschlossen: nicht kanonisiert (kein kanonischer Slug) |
| n-decane yield per n-hexanoic acid (Y decane), platinized Ti Type B | 52,3 ±6.9 | % | 95 % | extrahiert | "platinized Ti Type B (n=6) | 65.0±7.5 | 52.3±6.9 | 66.9±0.9" · cell=two-chamber, time=4 h, acids=["n-hexanoic acid"], electrode=platinized Ti Type B | Ausgeschlossen: nicht kanonisiert (kein kanonischer Slug) |
| n-decane yield per n-hexanoic acid (Y decane), Pt/Ir on Ti | 21,2 ±52.6 | % | 95 % | extrahiert | "Pt/Ir on Ti (n=3) | 31.2±67.6 | 21.2±52.6 | 49.9±17.5" · cell=two-chamber, time=4 h, acids=["n-hexanoic acid"], electrode=Pt/Ir on Ti | Ausgeschlossen: nicht kanonisiert (kein kanonischer Slug) |
| Coulombic efficiency for n-decane, one-chamber cell (pure Pt) | 41,9 ±3.4 | % | 95 % | extrahiert | "CEdecane is significantly higher in the two-chamber setup (CEdecane=55.5±3.5 %, …" · cell=one-chamber, time=4 h, acids=["n-hexanoic acid"], electrode=pure Pt foil | Ausgeschlossen: nicht kanonisiert (kein kanonischer Slug) |
| Coulombic efficiency for n-hexanoic acid degradation (platinized Ti Type A) | 46,6 ±9.9 | % | 95 % | extrahiert | "including the second material that is based on platinized Ti (Type A, CEhexanoic…" · cell=two-chamber, time=4 h, acids=["n-hexanoic acid"], electrode=platinized Ti Type A | Ausgeschlossen: nicht kanonisiert (kein kanonischer Slug) |
| Coulombic efficiency for n-hexanoic acid degradation (CE hexanoic acid) | 93,1 ±6.7 | % | 95 % | extrahiert | "Platinized titanium performed best, achieving a coulombic efficiency (CE) of 93.…" · cell=two-chamber, time=4 h, acids=["n-hexanoic acid"], electrode=platinized Ti Type B | Ausgeschlossen: nicht kanonisiert (kein kanonischer Slug) |
| Coulombic efficiency for n-hexanoic acid degradation, one-chamber cell | 94,1 ±17.4 | % | 95 % | extrahiert | "This was confirmed for both one- and two-chamber setups, with a CEhexanoic acid …" · cell=one-chamber, time=4 h, acids=["n-hexanoic acid"], electrode=pure Pt foil | Ausgeschlossen: nicht kanonisiert (kein kanonischer Slug) |
| n-decane yield per n-hexanoic acid (Y decane), platinized Ti Type A | 60,4 ±43.0 | % | 95 % | extrahiert | "platinized Ti Type A (n=3) | 77.2±51.4 | 60.4±43.0 | 63.9±2.3" · cell=two-chamber, time=4 h, acids=["n-hexanoic acid"], electrode=platinized Ti Type A | Ausgeschlossen: nicht kanonisiert (kein kanonischer Slug) |
Extraktionspipeline
Rohextraktionen, Artefakte, Qualitätssignal
Extraktionsqualität
EhrlichkeitssignalBemessen Sie Ihr Vertrauen in die extrahierten Inhalte an diesen Signalen – so hat die Pipeline ihre eigene Ausgabe für diese Publikation bewertet.
Mittlere Parameterkonfidenz
92 %
Durchschnittliche Konfidenz der oben angezeigten PaperParameter-Zeilen
vor dem Zitieren mit dem Quell-PDF abgleichen · Werte 0–1
Diagramm-Explorer
Verändern Sie die Eingaben dieser Publikation und sehen Sie, wie sich das vorhergesagte Ergebnis verschiebt.
Modell erkunden
Der Reaktor in 3D, mit Strömung, die sich ein- und ausschalten lässt.
KI-Erkenntnisse
Widersprüche, Lücken und Chancen aus dem Vergleich dieser Publikation mit dem Korpus.
Ähnliche Publikationen vergleichen
Die nächsten Publikationen nach System, Materialien und Organismen, mit ihren Ergebnissen nebeneinander.
Quell-PDF
Die Publikation, wie sie erschienen ist.
Dieser Publikation ist noch kein 3D-Modell zugeordnet. Die daraus extrahierten Werte stehen unter „Extrahierte Werte“.
Schlagwörter
- Kolbe electrolysis
- Coulombic efficiency
- anode materials
- electrode lifetime
- aqueous electrolyte solutions
- cost-effectiveness
- liquid fuel production
Zitieren
Katharina Neubert, Matthias Schmidt, Falk Harnisch (2021). Platinized Titanium as Alternative Cost‐Effective Anode for Efficient Kolbe Electrolysis in Aqueous Electrolyte Solutions. ChemSusChem. https://doi.org/10.1002/cssc.202100854
- Zeitschrift
- ChemSusChem